杜 敏,李新平,陈立红,王志杰,李鸿魁.酶预处理对漂白针叶木浆性能和打浆能耗的影响[J].中国造纸学报,2015,30(2):22-28 本文二维码信息
二维码(扫一下试试看!)
酶预处理对漂白针叶木浆性能和打浆能耗的影响
Effect of Enzymatic Pretreatment of BSKP on Its Refining and Paper Properties
  
DOI:10.11981/j.issn.1000-6842.2015.02.22
中文关键词:  纤维素酶  漂白硫酸盐针叶木浆  预处理  打浆  强度性能
Key Words:cellulase  bleached softwood kraft pulp  pretreatment  refining  paper properties
基金项目:国家自然科学基金面上项目(31370578);陕西省科技厅省级重点实验室项目(2011HBSZS014);陕西省科技厅自然科学基础研究项目(2014JZ013);陕西科技大学博士启动基金项目(BJ13-21)。
作者单位
杜 敏1 1.陕西科技大学轻工与能源学院,陕西省造纸技术及特种纸品开发重点实验室, 陕西西安, 710021 
李新平1 1.陕西科技大学轻工与能源学院,陕西省造纸技术及特种纸品开发重点实验室, 陕西西安, 710021 
陈立红2 2.陕西科技大学化学与化工学院, 陕西西安, 710021 
王志杰1 1.陕西科技大学轻工与能源学院,陕西省造纸技术及特种纸品开发重点实验室, 陕西西安, 710021 
李鸿魁1 1.陕西科技大学轻工与能源学院,陕西省造纸技术及特种纸品开发重点实验室, 陕西西安, 710021 
摘要点击次数: 4064
全文下载次数: 1616
中文摘要:
      采用纤维素酶对漂白针叶木浆进行预处理,研究了酶预处理对浆料打浆性能和成纸强度性能的影响。结果表明,酶预处理后,漂白针叶木浆纤维的表面起毛且长度减小,细小纤维含量增加。对酶预处理后浆料进行PFI磨打浆,当打浆5000或10000转时,随着酶用量的增加,浆料游离度逐渐降低,表明酶预处理可降低打浆能耗,但打浆过程中纤维易被切断。打浆与适当的酶预处理相结合,可提高成纸强度性能,当打浆500、2000和5000转时,酶用量为0.01 U/g浆料的成纸抗张指数较未经酶预处理浆料分别提高了54.6%、60.3%和48.5%。
Abstract:
      A cellulase was used to pre-treat bleached softwood kraft pulp (BSKP) in present study, the changes of fiber morphology,freeness of pulp in refining and paper properties were investigated,and the effects of enzymatic pretreatment on refining and paper properties were studied.The results showed that when the BSKP was pre-treated by the cellulase, fiber surface was of hairiness, fiber length decreased, and the fines content increased, which was similar to the effect of refining. When enzymatic pre-treated BSKP refined at PFI mill for 5000 r or 10000 r, the pulp freeness decreased with the enzyme dosage increasing. Enzymatic pretreatment could save refining energy significantly, but the pretreated fibers were easier to be cut in refining. Appropriate enzymatic pretreatment and refining could increase the physical strength of the paper. Comparing to the control samples, the paper tensile index improved by 54.6%, 60.3% and 48.5% when the pulps were pre-treated with enzyme dosage of 0.01 U/g and the pulps were refined for 500 r, 2000 r, and 5000 r in PFI mill respectively.